Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | Mixed 2:1; TM R050-36 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8010 psi | ASTM D638 |
Plaskolite West Optix® CA-945 Clear Impact Modified Acrylic Resin Impact modified acrylic resin, extrusion and injection moldingApplications: An impact-modified acrylic resin for extrusion and injection molding. This resin offers impact strengths up to six times .. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | ASTM D638 |
Nylene® 321 (HS) Impact Modified Nylon 6 Description: Nylene® 321 (HS) is an impact modified nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio.. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | TM R050-36 |
Resinlab® EP1330LV Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | TM R050-36 |
Resinlab® EP750 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP750 Clear is a two part unfilled epoxy structural adhesive which ingredients are listed in the Code of Federal Regulations Title 21 175.105 (Adhesives) and 175.300 (Resinous and polymer.. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PS-1000 Polybutylene Terephthalate (PBT)
(discontinued **) Description/Features:UL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 55.2 - 103 MPa | 8000 - 15000 psi | Average value: 74.7 MPa Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-50GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ NL-15KV/000 Nylon 6/12, Aramid Fiber
(discontinued **) Description/Features:Aramid Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8010 psi | |
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the m.. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8010 psi | ASTM Data |
Styron Pulse® 930 ABS + Polycarbonate PULSE® 930 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at room temperature. PULSE 930 Engineering resin has been used i.. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8010 psi | ASTM D638 |
Adell BI-10 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8010 psi | ASTM D638 |
Adell BI-30 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | ASTM D638 |
Applied Composites 8012 Polyester SMC Industry Application: SpecialtyProduct Application: Food EquipmentDistinct Features: NSF ApprovedInformation provided by Applied Composites Corporation. |
|||
Tensile Strength, Ultimate | 55.2 - 172 MPa | 8000 - 25000 psi | Average value: 113 MPa Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Tensile Strength, Ultimate | 55.2 - 123 MPa | 8000 - 17800 psi | Average value: 90.9 MPa Grade Count:24 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ MP-10GF/10T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 55.2 MPa | 8000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® UR-20CF/000 Thermoplastic Elastomer - TPU, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 55.2 - 210 MPa @Temperature -40.0 - 150 °C |
8010 - 30500 psi @Temperature -40.0 - 302 °F |
Average value: 87.1 MPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Tensile Strength, Ultimate | 55.2 - 68.9 MPa | 8000 - 10000 psi | ASTM D638 |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |