Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 52.1 MPa | 7560 psi | ISO 527-1, 2 |
Polyplastics Duranex® C7640 Polybutylene Terephthalate (PBT), Super low warpage, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |