Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 50.33 MPa | 7300 psi | |
Abatron AboCast 8-4/Abocure 8-4 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/60 ratio (pbw); Gel time, 100 g (3.5 oz.): 240 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adh.. |
|||
Tensile Strength, Ultimate | 50.33 MPa | 7300 psi | |
Abatron AboCast 8-15/Abocure 8-15 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/11.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 70 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |