Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 5.30 MPa | 769 psi | ASTM D638 |
Multibase Multi-Flex® TPE A 6900 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 5.30 MPa | 769 psi | ASTM D638 |
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 61 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e.. |
|||
Tensile Strength, Ultimate | 5.30 MPa | 769 psi | ASTM D638 |
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 56 MFI
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel.. |
|||
Tensile Strength, Ultimate | 5.30 MPa | 769 psi | ASTM D638 |
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 54 MFI
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel.. |
|||
Tensile Strength, Ultimate | 5.30 MPa | 768 psi | |
Colorite Polymers Vinylbond 95-950-45 PVC Compound Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri.. |