Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 49.7 MPa | 7210 psi | ASTM D638 |
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag.. |