Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D638-95 |
Multibase Multi-Pro® 0505 RC Black 5.2% Glass Filled Polypropylene This product was specially designed for one customer's glass filled polypropylene application.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | |
Parylene Coating Services N Poly (P-Xylylene) Monomer is para-xylylene. Parylene N has a lower coefficient of friction and therefore is recommended where lubricity is needed. Parylene N exhibits a slight haze at thicknesses over 5 microns.Par.. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D638 |
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | TM R050-36 |
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor.. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D412 |
PB1000-650 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | 0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638 |
Americas Styrenics STYRON™ 666LR General Purpose Polystyrene Resin
(discontinued **) STYRON™ 666LR is a medium flow general purpose polystyrene specifically designed to blend with styrene butadiene styrene block copolymers for packaging applications requiring high clarity, improved.. |
|||
Tensile Strength, Ultimate | 44.8 - 110 MPa | 6500 - 16000 psi | Average value: 74.2 MPa Grade Count:32 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Tensile Strength, Ultimate | 44.8 - 131 MPa | 6500 - 19000 psi | Average value: 55.4 MPa Grade Count:15 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D638-95 |
Multibase Multi-ABS 801 Natural Extrusion Grade Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM Data |
Styron Pulse® 600 ABS + Polycarbonate PULSE® 600 Engineering resin is designed to offer a superior balance of properties between impact strength, heat resistance and processability. It offers excellent processability, medium heat res.. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM Data |
Styron Pulse® 830 ABS + Polycarbonate PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.PULSE 830 Engineering resin has been used in automot.. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | |
Elastomer Engineering E900-90A Polyurethane A polyether-based urethane that is excellent in water treatment applications. Typical uses: Wheels, casters, rolls, metal forming strippers and pads. Information provided by Elastomer Engineering I.. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D412 |
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D412 |
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D638 |
Ecomass® 1050ZB92 Filled Polyamide Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyGood ToughnessInformation provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D638 |
Ecomass® 1700TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyRigidInformation provided by Technical Po.. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D638 |
Ecomass® 1850ZG90 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D638 |
Ecomass® 1850ZG92 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | |
Cotronics Duralco™ 120 500°F Silver Filled Epoxy, Electrically Conductive Contains over 70% ultra fine silver to provide excellent electrical conductivity. Cures at room temperature.>Applications: ideal for use where maximum conductivity is required. |
|||
Tensile Strength, Ultimate | 44.8 MPa | 6500 psi | ASTM D412 |
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Tensile Strength, Ultimate | 44.8 - 160 MPa | 6500 - 23200 psi | Average value: 87.1 MPa Grade Count:21 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |