Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 41.0 - 70.0 MPa | 5950 - 10200 psi | Average value: 55.1 MPa Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
Kleerdex Kydex® 130 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Decorative thermoplastic sheetApplications: Appliances, laminations, electronics, in-store displays, medical devices, equipment housings, dental equipmentFeatures: For deep to hard to form parts or .. |
|||
Tensile Strength, Ultimate | 41.0 - 58.0 MPa | 5950 - 8410 psi | Average value: 50.1 MPa Grade Count:10 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
IDI Composites 44-1 Thermoset Polyester, Molding Multi-purpose medium strength material with excellent moldability and low cost.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
IDI Composites 44-10 Thermoset Polyester, Molding Multi-purpose medium strength material with excellent surface appearance, corrosion resistance, and V-O flame resistance.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
Hannam Chemical Hanalac 740 ABS, Super High Impact Grade Superior impact strength, even at low temperature. Applications: helmets, shoe heels, bobbins, roller skates, bags, pipes, radiator grills, auto parts, appliance wheels. |
|||
Tensile Strength, Ultimate | 41.0 MPa @Temperature 1149.0 °C |
5950 psi @Temperature 2100.2 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | |
Haysite 14200 Polyester BMC, 15% Glass Reinforced The 14200 series bulk molding compound is one of Haysite's newest molding compound families. This grade can be compression, transfer, or injection molded. Good mechanical strength and exceptional a.. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | |
Haysite H254 Polyester Laminate Solder Pallet and Work Holder Sheet A Static dissipative sheet material for use in electronic assembly. Resistant to hot solder and solvents. Standard color is blue/grey. Available thicknesses from.. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
Sumitomo Bakelite North America 4064 Mineral Filled Electrical Encapsulation Grade Epoxy Rogers electrical encapsulation grade epoxy is recommended for capacitors, resistors, gold lead encapsulation, relays, coils and bobbins.Information provided by Sumitomo Bak North America, Inc. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | DIN 53504 |
Lubrizol ESTANE® X1014 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
Plenco 08235 Polyester BMC, Compression Molded PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable .. |
|||
Tensile Strength, Ultimate | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
Cosmic Plastics K77 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
Plenco 6343 Phenolic, Granular, Transfer Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Tensile Strength, Ultimate | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
Cosmic Plastics D69 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ISO 527-1, 2 |
Polyplastics Duracon® TD-15 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ISO 527 |
DSM Fibre Intermediates Nyrim® 2025 (Wollastocoat®), Dry Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5940 psi | after optimum cure |
Armstrong C-7/W Epoxy Adhesive, 1:1 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ATSM D638 |
Ashley Polymers Ashlene® 940H Nylon 11 A general purpose highly flexible natural Nylon 11 resin with UV stabilizers.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
Chem Polymer Chemlon 275 Nylon 6, Copolymer Impact Modified An extrusion grade nylon 6 copolymer that provides excellent melt strength, impact, tensile elongation and flexibility.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ATSM D638 |
Ashley Polymers Ashlene® 925-20PF Nylon 12, PTFE Lubricated 20% filled PTFE lubricated, Nylon 12.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | Dynamic tensile strength |
Channel Industries 5400 Lead Zirconate Titanate Piezoelectric Navy Type ICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extens.. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D651 |
Resinoid 2010 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Tensile Strength, Ultimate | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
Plenco 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 302 is a two-stage, woodflour and flock-filled phenolic molding compound. It has low specific gravity, broad molding latitude and an excellent balance of electrical and physical properties... |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | ASTM D638 |
Plaslok 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 302 is a two-stage, woodflour and flo.. |
|||
Tensile Strength, Ultimate | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 41.0 MPa | 5950 psi | |
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |