Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 4.80 MPa | >= 696 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 7150 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 4.80 MPa | 696 psi | ASTM D412 |
Multibase Multi-Flex® TPE G 7150 BLK Multi-Flex® G 7150 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactu.. |
|||
Tensile Strength, Ultimate | 4.80 MPa | 696 psi | ASTM D638 |
ExxonMobil Escorene® UL-7750 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Tensile Strength, Ultimate | 4.80 MPa | 696 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 4002 BLK Multi-Flex® A 4002 is based on Shell's Kraton G polymer and is suitable for soft touch applications for the automotive industry. It exhibits excellent paintibility adhesion. Multi-Flex TPE cont.. |