Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 386.1 MPa @Temperature 204 °C |
56000 psi @Temperature 399 °F |
|
ATI Allegheny Ludlum AL 468™ Dual Stabilized- Low Titanium Stainless Steel Characteristics:good corrosion resistance in a wide range of environments, can be used in annealed cold formed or as-welded conditions. Applications: used in place of Type 304 in an oxidizing when .. |