Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 37.5 MPa
5440 psi
ASTM D412
BASF Elastollan® 695A15N Polyester Type Polyurethane Elastomer
This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes..
Tensile Strength, Ultimate 37.5 MPa
5440 psi
ASTM D638-95
Multibase Multi-ABS 3525 Black
Moisture content is 0.08%.Data provided by Multibase.
Tensile Strength, Ultimate 37.5 MPa
5440 psi
ASTM D412
BASF Elastollan® 695A15 Polyester Type Polyurethane Elastomer
This grade contains a hydrolytic stabilizer. The Elastollan 600 Series of products listed are products that are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are ..