Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 359 MPa | 52000 psi | |
Pacific Sintered Materials SS-316-SH 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 359 MPa | 52000 psi | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-SH Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 359 MPa @Temperature 816 °C |
52100 psi @Temperature 1500 °F |
|
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, welded and tested as welded Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Tensile Strength, Ultimate | 359 MPa | 52000 psi | Longitudinal |
Special Metals Electroformed Nickel, 200 Micron (8 mil) Foil, Electroformed and Annealed Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52100 psi | |
Alcoa Deltalloy® 4032-T651 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = C (A = best; E = worst). General 4032 characteristics and uses: Good machinability and drilling characterist.. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52000 psi | |
Eagle Brass 110 EPT COPPER, Extra Spring Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Ultimate | 359 - 448 MPa | 52000 - 65000 psi | |
Eagle Brass 18665 MSP1, 1/4 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Ultimate | 359 - 427 MPa | 52000 - 62000 psi | |
Eagle Brass 19210 XP-10 Copper Iron, 3/4 Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Ultimate | 359 - 427 MPa | 52000 - 62000 psi | |
Eagle Brass 220 Commercial Bronze, 3/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52000 psi | |
Eagle Brass 715 Copper Nickel 30%, Annealed 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Ultimate | 359 MPa @Temperature 482 °C |
52000 psi @Temperature 900 °F |
|
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536 Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu.. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52000 psi | |
Eagle Brass 101 OFE COPPER (Certified), Extra Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52000 psi | |
Eagle Brass 102 OF COPPER (Non-Certified), Extra Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Ultimate | 359 MPa | 52100 psi | In rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Ultimate | 359 MPa | 52100 psi | In rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Ultimate | 359 MPa | 52100 psi | In rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Ultimate | 359 MPa | 52100 psi | In rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Ultimate | 359 MPa | 52100 psi | In rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Ultimate | >= 359 MPa | >= 52100 psi | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Dent Resistant (DR 210) Compared to DS Type B, DR steels have higher initial YS which contributes to increased strength after forming.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 359 - 448 MPa | 52100 - 65000 psi | |
Ametek High Purity Nickel Strip 899L Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 359 - 448 MPa | 52100 - 65000 psi | |
Ametek High Purity Nickel Strip 899M Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 359 MPa | 52100 psi | In rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Ultimate | 359 MPa | 52100 psi | |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Steel, Bake Hardenable (BH 210) Brake Hardenable steels offer good formability and an increase in strength after paint bake.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 359 - 448 MPa | 52100 - 65000 psi | |
Ametek High Purity Nickel Strip 899A Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 359 MPa @Temperature 593 °C |
52100 psi @Temperature 1100 °F |
0.059" Coil |
AK Steel 15 Cr-Cb® ULTRA FORM® Ferritic Stainless steel AK Steel’s 15 Cr-Cb ULTRA FORM® is a low-carbon, low-nitrogen ferritic grade of stainless steel with an intermediate, 14.5% chromium content. Alloying additions of Ti, Cb, Si and Mn provide excell.. |