Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | temp |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 34.5 - 91.0 MPa | 5000 - 13200 psi | Average value: 58.1 MPa Grade Count:23 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Ultimate | 34.5 - 160 MPa | 5000 - 23200 psi | Average value: 75.2 MPa Grade Count:26 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Tensile Strength, Ultimate | 34.5 - 44.8 MPa | 5000 - 6500 psi | Average value: 39.5 MPa Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 34.5 - 300 MPa | 5000 - 43500 psi | Average value: 118 MPa Grade Count:164 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Tensile Strength, Ultimate | 34.5 MPa @Temperature 260 °C |
5000 psi @Temperature 500 °F |
ASTM D638 |
Saint-Gobain Meldin® 7021 Direct Formed Graphite Filled Polyimide Finished parts and basic shapes made from 15% by weight graphite filled polyimide material for applications high wear resistance, good thermal oxidative stability, and high temperature resistance. .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 275 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 9095 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 9450P ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM Data |
Styron Magnum™ 213 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D638 |
Ecomass® 1050TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Techn.. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D638 |
Ecomass® 1066ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D638 |
Ecomass® 1080ZB92 Filled Polyamide Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyExcellent ToughnessInformation provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | |
Cotronics Bond-It™ 7040 Epoxy, Room Temperature Cure Forms high strength bonds to difficult metals, plastics, glass, ceramics, composites, etc. Cures at room temperature with high temperature strength and good electrical and thermal shock resistance... |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 1403 Electrical Grade BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties An.. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose materia.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Tensile Strength, Ultimate | 34.5 - 55.2 MPa | 5000 - 8000 psi | |
Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, .. |
|||
Tensile Strength, Ultimate | 34.5 - 48.3 MPa | 5000 - 7000 psi | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Tensile Strength, Ultimate | 34.5 - 68.9 MPa | 5000 - 10000 psi | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Tensile Strength, Ultimate | 34.5 - 55.2 MPa | 5000 - 8000 psi | |
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D412 |
Lubrizol Estane® 2103-80AEF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product l.. |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D412 |
MF-5040 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 34.5 MPa | 5000 psi | ASTM D412 |
MF-5056 Polyurethane-based Biomedical Elastomer |