Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D638 |
Global B-5200 High Density Polyethylene Description-has excellent stiffness thus requires less material to make
blow moldingApplications-food containers, drinking bottles, medicine bottles, water containersInformation provided by Global .. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D638 |
Global B-6200 High Density Polyethylene Description-suitable for high quality blow molding, provides excellent surface glossiness in combination w/ outstanding environmental stress cracking resistanceApplications-cosmetics bottles, shampo.. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
SK Chemicals SKYTHANE® 180A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
SK Chemicals SKYTHANE® 185A L series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
SK Chemicals SKYTHANE® S385A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
SK Chemicals SKYTHANE® S180A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
Lubrizol Estane® S180A Thermoplastic Polyurethane Type: Estane® S180A is a Shore 83A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mi.. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
Lubrizol Estane® S385A Thermoplastic Polyurethane Type: Estane® S385A is a Shore 85A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi.. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
Lubrizol Estane® T365A Thermoplastic Polyurethane Type: Estane® T365A is a Shore 70A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
Lubrizol Estane® X-590A-2FR Thermoplastic Polyurethane Type: Estane® X-590A-2FR TPU is a Shore 89A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
Lubrizol Estane® CS190A Thermoplastic Polyurethane Type: Estane® CS190A is a Shore 90A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Ultimate | 34.3 MPa @Temperature 260 °C |
4970 psi @Temperature 500 °F |
ASTM D1708 |
Daelim H&L Plavis-G15 CM 15% Graphite Filled Aromatic Polyimide Bearing Compression Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to.. |
|||
Tensile Strength, Ultimate | 34.3 MPa @Temperature 260 °C |
4970 psi @Temperature 500 °F |
ASTM D1708 |
Daelim H&L Plavis-G15 ISO 15% Graphite Filled Aromatic Polyimide Bearing Isostatically Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded .. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4970 psi | ASTM D638 |
Colorite Polymers 1066 Non-Phthalate 66 Series Vinyl Compound Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phth.. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D412 |
SK Chemicals SKYTHANE® 385A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D638 |
Samyang Triel® 5650 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5650 is an extrusion grade.Information provided by Samyang. |
|||
Tensile Strength, Ultimate | 34.3 MPa | 4980 psi | ASTM D638 |
Samyang Triel® 5652EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5652EM is an extrusion grade.Information provided by Samyang. |