Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 317 MPa | 46000 psi | |
PSM Industries Pacific Sintered Metals Bronze BT-126 Powdered Metal Higher strength structural and bearing bronzeInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 317 - 386 MPa | 46000 - 56000 psi | |
Eagle Brass 210 Gilding Metal, 3/4 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Ultimate | 317 - 386 MPa | 46000 - 56000 psi | |
Eagle Brass 510 Phosphor Bronzes 5% A, Annealed Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Ultimate | 317 - 400 MPa | 46000 - 58000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | 317 - 372 MPa | 46000 - 54000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, Annealed 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | 317 MPa | 46000 psi | Worked |
CMW® D54F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 317 MPa | 46000 psi | |
AK Steel Cold Rolled Carbon Steel, Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 317 MPa | 46000 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F) steels are made by adding titanium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 317 MPa | 46000 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Deep Drawing Steel (DDS Type B), Standard Grade DDS may be used in drawing applications.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 317 MPa | 46000 psi | |
AIM 62Sn/Pb36/Ag2 Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | 317 MPa | 46000 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Drawing Steel (DS Type B), Standard Grade DS Type B may be used in drawing applications.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 317 MPa | 46000 psi | |
Pacific Sintered Materials BT-126 Bronze Powdered Metal Applications: Higher strength structural and bearing bronze.All information provided by Pacific Sintered Metals. |