Polymer Property : Tensile Strength, Ultimate = 315 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 315 MPa

@Temperature 760 °C
45700 psi

@Temperature 1400 °F
Haynes 25 alloy, vacuum investment castings, solution treated
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..