Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 303 MPa | >= 43900 psi | |
Alcoa UltrAlloy® 6020-T8 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
Tensile Strength, Ultimate | 303 - 372 MPa | 44000 - 54000 psi | |
Eagle Brass 230 Red Brass, 1/4 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Ultimate | 303 - 372 MPa | 44000 - 54000 psi | |
Eagle Brass 240 Low Brass, Annealed CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Ultimate | 303 MPa | 43900 psi | ASTM D638/D412 |
Covestro Baydur® STR/C-410 IMR Polyurethane Composite SRIM Foam, 60% Glass Filled, MDI-based 2-Component Liquid System Contains continuous strand fiberglass mat.0.126 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer .. |
|||
Tensile Strength, Ultimate | 303 MPa | 43900 psi | |
AK Steel Cold Rolled Carbon Steel, Drawing Steel (DS Type B), Standard Grade DS is made by adding aluminum to the molten steel and may be used in drawing applications.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 303 MPa | 43900 psi | |
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 303 MPa | 43900 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F®) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 303 MPa | 43900 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or columbium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel |