Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3000 MPa | 435000 psi | |
Honeywell Spectra® 1000 Fiber Spectra® fiber 1000, the second in a series of Spectra® fibers, was developed to meet customers’ needs for increased performance. It is available in a multitude of deniers for use in a wi.. |
|||
Tensile Strength, Ultimate | 3000 MPa | 435000 psi | |
UBE Tyranno Grade F Ceramic Semi-Conductive Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Tensile Strength, Ultimate | 3000 MPa | 435000 psi | Breaking Tenacity |
DuPont™ Kevlar® 49 Aramid Fiber 1140 Denier; 768 Filaments. Kevlar® 49 is a high-modulus type used primarily in fiber optic cable, textile processing, plastic reinforcement, ropes, cables, and composites for marine sporting good.. |
|||
Tensile Strength, Ultimate | 3000 MPa | 435000 psi | |
China Tungsten YG12 Tungsten Carbide Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 3000 MPa | 435000 psi | |
China Tungsten YG18C Tungsten Carbide Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 3000 MPa | 435000 psi | |
Teijin Technora® Fiber Technora® is a Teijin registered trademark. |