Polymer Property : Tensile Strength, Ultimate = 3.73 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.73 - 125 MPa

@Temperature -40.0 - 160 °C
541 - 18100 psi

@Temperature -40.0 - 320 °F
Average value: 53.1 MPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Tensile Strength, Ultimate 3.73 - 125 MPa

@Strain 0.250 - 10.0 %
541 - 18100 psi

@Strain 0.250 - 10.0 %
Average value: 53.1 MPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Tensile Strength, Ultimate 3.73 MPa
541 psi
Momentive Performance Materials RTV162 White Adhesive Sealant, Non-Corrosive Paste
One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Non-corrosive bindi..