Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.10 MPa | 450 psi | ISO 37 |
Multibase TPSiV® 4000-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Tensile Strength, Ultimate | 3.10 MPa | 450 psi | TPE-0153 (ASTM D 412) |
ExxonMobil Santoprene® 8211-35W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
Tensile Strength, Ultimate | 3.10 MPa | 450 psi | ASTM D638 |
ExxonMobil Escorene® LD-737 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.5% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications. |
|||
Tensile Strength, Ultimate | 3.10 MPa | 450 psi | |
Dow Corning HS II BASE & 10:1 CLAY CATALYST High strength silicone mold making rubber, suited for the art foundry industry that typically uses sulfur-based clays. HS II Base with HS II 10:1 Clay Catalyst is recommended for use with polyesters.. |
|||
Tensile Strength, Ultimate | 3.10 MPa | 450 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |
|||
Tensile Strength, Ultimate | 3.10 MPa | 450 psi | Cured property; ASTM D412 |
Aptek 2214-A/B Low modulus urethane ESD coating/adhesive Space Grade, Low modulus urethane ESD coating/adhesiveAPTEK is a carbon-filled, thixotropic, two component, electrically conductive, flexible urethane coating/adhesive designed to dissipate an elect.. |
|||
Tensile Strength, Ultimate | 3.10 MPa | 450 psi | TM R050-36 |
Resinlab® SEC1233 Silver Filled Epoxy Adhesive Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit.. |