Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | ASTM D638-61T |
Rotuba 856, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | ASTM D638 |
NCMT NanoPAC™ HG602 High Performance Polypropylene Nanocomposite Applications: Household Industry Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Tensile Strength, Ultimate | 27.0 MPa @Temperature 90.0 °C |
3920 psi @Temperature 194 °F |
ISO 527 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Tensile Strength, Ultimate | 27.0 - 156 MPa | 3920 - 22600 psi | Average value: 87.9 MPa Grade Count:87 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Tensile Strength, Ultimate | 27.0 - 33.0 MPa | 3920 - 4790 psi | Average value: 29.0 MPa Grade Count:3 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | |
Freudenberg Simrit Superiorâ„¢ F850 Fluoroelastomer Cost-effective, high performance compound for semiconductor applications. Superior F850 offers outstanding plasma resistance and low particulation in a wide range of plasma environments. |
|||
Tensile Strength, Ultimate | 27.0 MPa @Temperature 22.0 °C |
3920 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of .. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | |
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA) High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren.. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3910 psi | |
Shinil Chemical SHINNANO PP Polymer Nanocomposite Door Trim SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | ISO 527-1, 2 |
Polyplastics Duracon® TD-35 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3910 psi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 250 FT EB Thermoplastic Vulcanizate Neoplast 250 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | DIN 53504 |
Lubrizol ESTANE® 58565 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | ISO 527-1 |
Chengdu Polyster H4543 Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and injection grade. Contains improved color- stable antioxidants. Applications requiring high original color retention. Molded and injected products for consumer use, such as se.. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | |
Covestro Baydur® GS PIR A Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | ISO 527 |
Eastman Eastar GN071 Natural PETG Copolyester EASTAR GN071 Copolyester is used for injection molding applications. It is sparkling clear, tough, chemical resistant, odor free, versatile, easy to work with and affordable. Cleaning solutions wi.. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman ComAlloy Voloy® 100 Polypropylene, Mineral Reinforced, Flame Retardant, UL, CSA Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 27.0 - 35.0 MPa | 3920 - 5080 psi | ISO 527 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3920 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 27.0 - 63.0 MPa | 3920 - 9140 psi | Average value: 39.5 MPa Grade Count:20 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | <= 27.0 MPa | <= 3920 psi | With carbon black or gum stocks. ASTM D412-80 |
DuPont Performance Polymers Hypalon® HPG-6525 Chlorosulfonated Polyethylene Rubber, General Description
(disc Product form is white, odorless chips. Distinguishing Feature: High viscosity polymer. Good low temperature and heat resistance. Good processing at high extensions.27 % Chlorine Content. 1% Sulf.. |