Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 245 MPa @Temperature 980 °C |
35500 psi @Temperature 1800 °F |
|
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Ultimate | 245 MPa | 35600 psi | |
Shinil Chemical SHINCON PEEK-CF LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Tensile Strength, Ultimate | 245 MPa | 35500 psi | 5mm/min; ISO 527 |
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Dry) Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil.. |
|||
Tensile Strength, Ultimate | >= 245 MPa | >= 35500 psi | Guaranteed Minimum L-T Direction |
Aleris HOGAL 5558 Aluminum 5026-O/H111 HOGAL 5558 is produced according to EN AW-5026.Information provided by Aleris. |
|||
Tensile Strength, Ultimate | 245 MPa @Temperature 982 °C |
35500 psi @Temperature 1800 °F |
|
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |