Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | DIN 53455 |
Polikim ULPOLEN® 1000 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | DIN 53455 |
Polikim ULPOLEN® 300 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | DIN 53455 |
Polikim ULPOLEN® 500 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | DIN 53455; ASTM D638 |
Kolon KOPEL® KP3340 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D638 |
KKPC Kuhmo HF400 Flame Retarded General Purpose HIPS Key features: Translucent Injection. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resista.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D638 |
KKPC Kuhmo HF401 Flame Retarded General Purpose HIPS Key features: High-fluidity. Common Uses: Office appliances.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resistance and h.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D638 |
KKPC Kuhmo HFH 403 Flame Retarded HIPS Key features: Low flammable V-2 grade. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resis.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D638 |
KKPC Kuhmo HFH 405 Flame Retarded HIPS Key features: Non-halogen type. Common Uses: Parts needing non-halogen type.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | |
Shinil Chemical SHINNANO PP Polymer Nanocomposite IP SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | |
Shinil Chemical SHINSTRA PP SE3501 Structural Polymer Bumper SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D412 |
SK Chemicals SKYTHANE® 865A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D412 |
SK Chemicals SKYTHANE® T865A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D412 |
SK Chemicals SKYTHANE® UB410 Powder Coating Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D412 |
SK Chemicals SKYTHANE® 410 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D412 |
Lubrizol Estane® T370A Thermoplastic Polyurethane Type: Estane® T370A is a Shore 74A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3550 psi | ISO 527 |
Lubrizol Estane® ZHF 82AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 82AT0 NAT021 is an 82A aromatic polyether-based, non-halogen flame retardant, thermoplastic polyurethane (TPU) compound.Features: Soft, matte finished, good flame retardant proper.. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3550 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8440 Polyolefin Elastomer Description: Engage® 8440 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It is an excellent thermoplastic elastomer .. |
|||
Tensile Strength, Ultimate | 24.5 MPa | 3560 psi | ASTM D638 |
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang. |