Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | ASTM D638 |
Multibase Multi-Pro® 4615 X White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 22.8 - 27.6 MPa | 3300 - 4000 psi | ASTM D638 |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3310 psi | ASTM D638 |
Rostone Rosite® 4950BS SMC Thermoset Polyester, 10% Glass Reinforced
(discontinued **) Key Features: Low Shrink; Tight DimensionsRemarkable physical and electrical strength combined with excellent dimensional stability. Information provided by Oneida-Rostone Group. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3310 psi | ASTM D4745 |
3M Dyneon™ CC144/S PTFE, 40% Bronze Filled
(discontinued **) Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | Vulcanized |
KKPC KOSYN 1724 Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | Vulcanized |
KKPC KOSYN 1778K Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | |
KKPC KOSYN SOL 5990 Solution Styrene Butadiene Rubber (S-SBR) Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It .. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | ASTM D638 |
Techmer ES Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Carbon Filled Conductive Carbon, Powder Modified |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | |
Williams Advanced Alloys WS213 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | >= 22.8 MPa @Thickness 3.17 mm |
>= 3300 psi @Thickness 0.125 in |
ASTM D638 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | ASTM D638 |
Colorite Polymers 9533 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | ASTM D638 |
Colorite Polymers 9609 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | |
Colorite Polymers 9611 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | |
Colorite Polymers 9612 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | |
Colorite Polymers 9811 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | |
Colorite Polymers 9812 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3310 psi | |
3M Jet-Weld™ TS-230 Adhesive A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly. Sprayable/extrudable grade with long set time ideal for bonding a wide variety of p.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3310 psi | ASTM D638 |
Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | TM R050-36 |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Tensile Strength, Ultimate | 22.8 MPa | 3300 psi | |
Sylvin Technologies 6055 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |