Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 20.009 MPa @Temperature 125 °C |
2902.1 psi @Temperature 257 °F |
Air age, 70 hours; ASTM D412 Die C |
Freudenberg Simrit N475 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |