Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.18 MPa | 316 psi | ASTM D638 |
Multibase Multi-Flex® A 0840 Black TPE Thermoplastic Elastomer Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |