Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1860 MPa | 270000 psi | 3 in bar |
Carpenter Pyrotough® 78 Hot Work Die Steel Pyrotough® 78 alloy is a premium quality hot work die steel engineered to withstand the operating temperatures and pressures associated with die casting and hot extrusion operations. The patented c.. |
|||
Tensile Strength, Ultimate | 1860 MPa | 270000 psi | Oil Quenched from 871°C; 316°C Temper Temperature |
Latrobe Staminal™ Shock Resisting Die Steel Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, .. |