Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 176 MPa
25500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ SF-30CF/13T2S Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE/Silicone Lubricated &n
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 176 MPa
25500 psi
ATSM D638
Ashley Polymers Ashlene® 528L-30G Nylon 66, 30% Glass Reinforced
General purpose glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufacture..
Tensile Strength, Ultimate 176 MPa
25500 psi
ASTM D638
Chem Polymer Chemlon 133 G Nylon 66, 33% Glass Fiber Reinforced
A 33% glass fiber reinforced nylon 66 offering excellent high temperature performance, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer.
Tensile Strength, Ultimate 176 MPa
25500 psi
Osprey Metals CE13 Al-Si Controlled Expansion Alloy
Al-42%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.