Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 1590 MPa | >= 230000 psi | |
Kinetics MIM K3 Heat Treat K3 is a custom Mo-Fe alloy that provides improved fatigue properties over many other steel alloys while still maintaining good strength components, industrial or structural components and other appl.. |
|||
Tensile Strength, Ultimate | 1590 - 1600 MPa | 230000 - 232000 psi | |
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 5.75 in RCS Billet Size High Strength Alloy Steel LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi.. |
|||
Tensile Strength, Ultimate | 1590 MPa | 231000 psi | |
Specialty Materials 5505 Boron Epoxy Prepreg Tape Specialty Materials' 5505 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Exhibiting exceptional performance at temp.. |
|||
Tensile Strength, Ultimate | 1590 MPa | 231000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Tensile Strength, Ultimate | 1590 MPa @Temperature 316 °C |
230000 psi @Temperature 600 °F |
Tempering Temperature-800°F |
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
Tensile Strength, Ultimate | 1590 MPa | 231000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Tensile Strength, Ultimate | 1590 MPa | 230000 psi | Cold Worked 48% |
Latrobe MP159® Alloy MP159 is an alloy of the Multiphase family of alloys possessing the unique combination of ultra-high strength, ductility and corrosion resistance. Through work strengthening and aging, MP159 alloy .. |