Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 157 MPa | 22800 psi | |
Shinil Chemical SHINCON PEI-CNT Magazine Rack Magazine Rack is used to transfer, handle, and bake lead frame or PCB substrate in semiconductor and LED packaging assembly process. Current Metal Magazine is made of anodized aluminum which is exp.. |
|||
Tensile Strength, Ultimate | 157 MPa | 22800 psi | |
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Window Strip SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Tensile Strength, Ultimate | 157 MPa | 22800 psi | ASMT D638 |
Toyobo TS301 PPS, 30% Glass Fiber Reinforced Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo.. |
|||
Tensile Strength, Ultimate | 157 MPa | 22800 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 613 Nylon 6, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 157 MPa | 22800 psi | ASTM D638 |
A. Schulman ComAlloy Lubrilon® 636 Nylon 6/6, Carbon Fiber Reinforced, Proprietary Lubricant Package Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Tensile Strength, Ultimate | 157 MPa | 22800 psi | ISO value at 5mm/min. |
BASF Capron® 8232G HS FR 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant nylon 6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retard.. |
|||
Tensile Strength, Ultimate | 157 MPa | 22800 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 60G4 Nylon 66, 20% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |