Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Tensile Strength, Ultimate | 15.9 - 34.5 MPa | 2310 - 5000 psi | Average value: 28.3 MPa Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | ASTM D638 |
DuPont™ Surlyn® 9320W Ionomer Resin, Zinc
(discontinued **) Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | |
Freudenberg Simrit N470 Hydrocarbon Elastomer Nitrile Standard Nitrile is also known as Buna-N. Excelent resistance to petroleum-based oils and fuels, water and alcohols. Nitrile also has good resistance to acids and bases, except those with a strong o.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 8980-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 8999-95 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 9604-80 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 9812A-95 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 9925-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 5108 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Cytec EN-7 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Cytec EN-8 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | Molded property |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 5565 Heat Resistant Peroxide Cured FormulationNordel® IP 5565 |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D412 |
Colorite Polymers CS8039UL Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D412 |
Colorite Polymers CS9040UL--85B Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D638 |
Colorite Polymers 7077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D638 |
Colorite Polymers 7444D General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D638 |
Colorite Polymers 7500 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Colorite Polymers 7812 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D412 |
Colorite Polymers CS1537SC Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Dymax 3093 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Dymax 625 Structural Adhesive Structural Adhesives for Rugged Bonding, Sealing, Tacking and Potting in SecondsMulti-Cure® 600 Series products are rapid setting adhesives that cure by UV light, activator or heat. These products .. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | ASTM D638 |
Buckeye Polymers BP Flex D6707 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D638 |
Colorite Polymers 7002A-02 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | ASTM D412 |
BCC Products BC 8675E Polyurethane Elastomer BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2310 psi | 10 in/min; ASTM D412 |
PolyOne Elastamax XL-0257-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color.. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Sylvin Technologies 6147-83 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.9 MPa | 2300 psi | |
Colorite Polymers 7811 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |