Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 15.00 MPa | 2175 psi | |
Sylvin Technologies 8950-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.00 MPa | 2175 psi | |
Sylvin Technologies 9950-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |