Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1400 - 1430 MPa
203000 - 208000 psi
Latrobe Lescalloy® UT-18 VAC-ARC ; 2.125 in. round High Strength Alloy Steel
UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting..
Tensile Strength, Ultimate 1400 - 1410 MPa
203000 - 204000 psi
Latrobe Lescalloy® UT-18 VAC-ARC ; 3.75 in. round High Strength Alloy Steel
UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting..
Tensile Strength, Ultimate 1400 - 1600 MPa
203000 - 232000 psi
SSAB Tunnplat Docol® 1400 DP High-strength Steel
The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel ..
Tensile Strength, Ultimate 1400 MPa
203000 psi
Filament Property. Mat strength is 120 N/m
Cytec Thornel® Mat VMA Carbon Fiber
Data provided by the manufacturer, Amoco Performance Products, Inc.Composed of high strength, high modulus carbon filaments in a random-layered orientation. The fine diameter filaments are up to th..
Tensile Strength, Ultimate 1400 MPa
203000 psi
Filament Property. Mat strength is 120 N/m
Cytec Thornel® Mat VMC Carbon Fiber
Data provided by the manufacturer, Amoco Performance Products, Inc.Prepared by sectioning mat VMA into cubes ~ 0.5x0.5x1.0 in. VMC can be heterogeneously dispersed in matrix materials and thus enha..
Tensile Strength, Ultimate 1400 MPa
203000 psi
Filament Property. Mat strength is 120 N/m
Cytec Thornel® Mat VMD Carbon Fiber
Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 400 µm - adequate for good property improvement...
Tensile Strength, Ultimate 1400 MPa
203000 psi
Filament Property. Mat strength is 120 N/m
Cytec Thornel® Mat VME Carbon Fiber
Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 200 µm - inadequate for good mechanical property..
Tensile Strength, Ultimate 1400 MPa
203000 psi
Cytec Thornel® P-25 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.2000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 3.1 m/g yield..
Tensile Strength, Ultimate 1400 MPa
203000 psi
Cytec Thornel® P-25 4K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.4000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 1.4 m/g yield..
Tensile Strength, Ultimate 1400 MPa
203000 psi
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction + Aged 538°C (1000°F)/4hr/AC
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..