Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1345 MPa
195100 psi
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Ultimate 1345 MPa

@Temperature 95.0 °C
195100 psi

@Temperature 203 °F
Haynes 242® alloy, cold rolled sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Ultimate 1345 MPa
195100 psi
ATI Allvac® 718 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age
Data provided by Allvac.Applications: Jet engine rings, discs, shafts, compressor blades, seals, spacers. Fasteners, nuclear, oil & gas components.
Tensile Strength, Ultimate 1345 MPa
195100 psi
ATI Allvac® 718-OP® UNS N07718 Nickel Superalloy
Uses: Turbines and engines, fasteners, sub-surface safety valves, hot extrusion tooling, nuclear reactors.Property values are for samples in the metallurgical condition: 1800°F age.Information prov..
Tensile Strength, Ultimate 1345 MPa

@Temperature 371 °C
195100 psi

@Temperature 700 °F
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..
Tensile Strength, Ultimate 1345 MPa

@Temperature 316 °C
195100 psi

@Temperature 601 °F
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..
Tensile Strength, Ultimate 1345 MPa
195100 psi
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled
Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l..
Tensile Strength, Ultimate 1345 MPa
195100 psi
HP Alloys HPA COBALT Alloy 6BH, Wear Resistant, (Co-Cr-W) (UNS R30016)
Cobalt 6BH is the same composition of Cobalt 6B, except the material is hot rolled and then age hardened. The direct age-hardening after hot rolling provides the maximum hardness and wear resistance..