Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Nylene® 9533 , 33% Glass Reinforced Nylon 6/12 Description: Nylene® 9533 is a 33% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resou.. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® ES-30GF/000 Black Polyethersulfone (PESU) Edgetek™ ES-30GF/000 Black XP120031Information provided by PolyOne |
|||
Tensile Strength, Ultimate | 131 - 200 MPa | 19000 - 29000 psi | Average value: 170 MPa Grade Count:5 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Technetics Group Amicon™ PEEK 30% Carbon
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
IDI Composites 46-16-60 Thermoset Polyester, Sheet TRANSIT - A premium molding compound with excellent resistance to flame and smoke generation, high impact strength, and weatherability.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
IDI Composites M-209 Thermoset Polyester, Sheet MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p.. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Techmer ES Electrafil® J-50/CF/20 Polycarbonate, 20% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ISO 527-1, 2 |
Polyplastics Duranex® 7400F Polybutylene Terephthalate (PBT), Low friction, Low wear, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ATSM D638 |
Ashley Polymers Ashlene® 527-33G Nylon 66, 33% Glass Reinforced A 33% glass reinforced impact modified Nylon 66.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Chem Polymer Chemlon 130 GVH Nylon 66, 30% Glass Fiber Reinforced A glass fiber reinforced, flame retardant nylon 6,6 exhibiting excellent tensile strength and high temperature performance. The material has VO flammability rating according to UL94 testing procedu.. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Chem Polymer Durlex 740-10 GB PBT, 40% Short Glass Fiber, 10% Glass Bead Reinforced A 40% short glass fiber, 10% glass bead reinforced PBT, offering a combination of tensile strength, warpage control and dimensional stability for close tolerance applications.Data provided by the ma.. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ATSM D638 |
Ashley Polymers Ashlene® 520-33GU Nylon 66, 33% Glass Reinforced Nylon 66, 33% glass reinforced resin, utility grade for non-critical applications. Also available: 520S - 33GU Heat Stabilized, 520 - 33GBU Black, 520S - 33GBU Black with H.S.Data provided by the m.. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ATSM D638 |
Ashley Polymers Ashlene® 67MG Nylon 66, Glass/Mineral reinforced A glass/mineral reinforced Nylon 66 designed for high strength and dimensional stability.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
PolyOne Lubri-Tech™ NI-30GF/15T Nylon 6/10 - 30% Glass Fiber Reinforced - 15% PTFE Lubricated
(discontinued * Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications
&a Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
PolyOne Stat-Tech™ RA-06CF-09GF/000 EM Polyarylsulfone - ESD Applications - Flow Enhanced Grade
(discontinued Data provided by PolyOne. |