Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1265 MPa @Temperature 705 °C |
183500 psi @Temperature 1300 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Ultimate | 1265 MPa @Treatment Temp. 427 °C, Time 1.44e+7 sec |
183500 psi @Treatment Temp. 801 °F, Time 4000 hour |
Room temp test after thermal exposure |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |