Polymer Property : Tensile Strength, Ultimate = 1213 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1213 MPa
175900 psi
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®..
Tensile Strength, Ultimate 1213 MPa
175900 psi
Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1000°F [9.5 mm plate, transverse]
AK Steel 410 Cb Martensitic Stainless steel
AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved gra..