Tensile Strength, Ultimate 1210 MPa
175000 psi
Kinetics MIM 17-4PH Stainless Steel (H900 Condition)
Precipitation-hardening stainless steel. Offers a good balance between corrosion resistance and strength. Magnetic. Hardenable to various strength levels and hardness by varying the aging heat treat..
Tensile Strength, Ultimate 1210 MPa
175000 psi
Meehanite K-405 Austempered Ductile Iron
Type K-405 is for applications involving wear and requiring high tensile and endurance limit. Excellent founding properties enable more accurate castings with savings in machine stock required. Da..
Tensile Strength, Ultimate >= 1210 MPa
>= 175000 psi
H1050 Condition - 565°C
Latrobe Lescalloy® 13-8 Mo VIM-VAR Precipitation Hardening Stainless Steel
Lescalloy 13-8 Mo VIM-VAR is a precipitation hardening martensitic stainless steel offering excellent fracture toughness and transverse mechanical properties coupled with the resistance to stress-co..
Tensile Strength, Ultimate 1210 MPa
175000 psi
Precipitation Hardened
Special Metals NI-SPAN-C® Alloy 902
A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo..
Tensile Strength, Ultimate >= 1210 MPa
>= 175000 psi
Special Metals Nitinol High-Temperature Shape Memory Ni-Ti alloy Ribbon
Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology.
Tensile Strength, Ultimate 1210 MPa
175000 psi
Elgiloy® Co-Cr-Ni Alloy, Wire, 20% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..
Tensile Strength, Ultimate 1210 MPa
175000 psi
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 40% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Tensile Strength, Ultimate 1210 MPa
175000 psi
Cytec Thornel® P-120 Carbon Fiber/Epoxy Advanced Composite System