Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.5 - 110 MPa
1810 - 16000 psi
Average value: 75.0 MPa Grade Count:65
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Tensile Strength, Ultimate 12.5 MPa
1810 psi
ASTM D638
Multibase Multi-Flex® D 3902 MRS TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Tensile Strength, Ultimate 12.5 MPa
1810 psi
Heat aged 2 weeks at 175°C
DuPont Vamac® DP Activator OC Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
Tensile Strength, Ultimate 12.5 - 33.1 MPa
1810 - 4800 psi
Average value: 22.8 MPa Grade Count:5
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..