Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 1140 MPa | >= 165000 psi | Annealed and Aged |
IBC Advanced Alloys FA230 Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Tensile Strength, Ultimate | 1140 - 1250 MPa | 165000 - 181000 psi | Solution Annealed & Aged |
Materion Beryllium Copper Alloy 245C Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Tensile Strength, Ultimate | 1140 MPa @Temperature 315 °C |
165000 psi @Temperature 599 °F |
|
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Ultimate | 1140 - 1250 MPa | 165000 - 181000 psi | Solution Annealed & Aged |
Materion Beryllium Copper Alloy 245CT Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Tensile Strength, Ultimate | 1140 MPa | 165000 psi | |
Haynes 25 alloy, room temperature after 25% cold reduction, 1120°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Ultimate | 1140 MPa | 165000 psi | |
Haynes 625 alloy, plate after 1000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Ultimate | 1140 MPa | 165000 psi | |
Haynes 625 alloy, plate after 16000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Ultimate | 1140 MPa | 165000 psi | 593°C Temper Temperature |
Latrobe Lescalloy® 4340 VAC-ARC ; 10.5" square High Strength Alloy Steel LESCALLOY 4340 VAC-ARC steel is a low alloy, nickel-chromium-molybdenum steel capable of being heat treated to high strength levels. The alloy has a good combination of ductility, toughness and str.. |
|||
Tensile Strength, Ultimate | 1140 MPa | 165000 psi | Age Hardened |
Universal Wire Works Inconel 718 (AMS 5832) Filler Metal Inconel Filler Metal 718 is recommended for gas tungsten arc and gas metal arc welding of alloy 718, 706 and X-750. This double gamma prime alloy has excellent strength, good ductility up to 1300°F.. |
|||
Tensile Strength, Ultimate | 1140 MPa | 165000 psi | (hardened to 350 HB) |
Bohler-Uddeholm BÖHLER RAMAX® HH Modified 420F Chromium alloyed steelTypical applications for Ramax® HH are: holders and bolsters for plastic molds, plastic and rubber molds with low requirements on polishability, and dies for plastic extrusion.. |
|||
Tensile Strength, Ultimate | 1140 MPa | 166000 psi | Long. |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate, Solution Treated Annealed ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |