Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 113 MPa | 16400 psi | |
Shinil Chemical SHINFLAME PA-66 GF Flame Retardant Polymer Under Hood SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Tensile Strength, Ultimate | 113 MPa | 16400 psi | ISO 527-1, 2 |
Polyplastics Duranex® 3216 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 113 MPa | 16400 psi | ASTM D638 |
Toyobo T-400 Nylon, 15% Glass-Reinforced Key Feature: G.F. 15%Information provided by Toyobo Co., Ltd |
|||
Tensile Strength, Ultimate | 113 MPa | 16400 psi | ASTM D638 |
Tipco Tipcolene® SEB 400 - 40% Chemically Coupled Glass Fibers Polypropylene Homopolymer with High Heat Stability 40% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Ultimate | 113 MPa @Temperature 60.0 °C |
16400 psi @Temperature 140 °F |
ISO 527 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |