Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 11.0 MPa | >= 1600 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO 4107 BLK Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
3M Dyneon™ Aflas® FA-150L PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 253-36 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It ca.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PE 1313
(discontinued **) PRE-ELEC PE 1313 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 13.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Chevron Phillips KN 226B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Chevron Phillips KN 230 LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE 1017 Film Extrusion Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D4745 |
3M Dyneon™ CC085 PTFE, PPS-Filled
(discontinued **) Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Momentive Performance Materials TSE397 Translucent Adhesive Sealant, Semi-Flowable One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Non-corrosive adhes.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Sylvin Technologies 8600-65 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Sylvin Technologies 9950-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 11.0 MPa @Temperature 70.0 °C |
1600 psi @Temperature 158 °F |
ASTM D638 |
Borealis Borstar® HE6081 Black Track Resistant HD Polyethylene Based Compound for Jacketing of Fiber Optical Cable Borstar HE6081 is based on high-density polyethylene and has a specially designed additive package to give excellent track resistance. It is also well protected against UV degradation in order to e.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Westlake EC483 Low Density Polyethylene WESTLAKE low-density polyethylene EC483 is recommended for use in the boardstock coating industry. This resin has low neck-in, good heat sealing properties, and good drawdown characteristics.Applica.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Ecomass® 4702ZB92 Filled Polyurethane Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Ecomass® 4703ZG92 Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Cytec EN-2521 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Dow HDPE 25455N High Density Polyethylene DOW HDPE 25455N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and gloss with excellent toughness. This resin has good processability over a.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | |
Dow LDPE 722M Low Density Polyethylene DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include c.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D412 |
Colorite Polymers Weatherflex™ CS1534WX (NTL01P) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Colorite Polymers 92-623A General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 2080 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Colorite Polymers 6000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman Rexell® H2103 Injection Molding LLDPE
(discontinued **) Linear-low medium density homopolymer, injection molding, FDA compliant.Features: Good ESCR, low taste and order.Applications: Containers, closures, and ideal for blends and non-carbonated beverage .. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Colorite Polymers 6574 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ASTM D638 |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |
|||
Tensile Strength, Ultimate | 11.0 - 14.0 MPa | 1600 - 2030 psi | Average value: 12.5 MPa Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Sheet/Profile extrusions". Each property range of values reported is mi.. |
|||
Tensile Strength, Ultimate | 11.0 MPa | 1600 psi | ISO 527 |
LATI LATISTAT 48/9900-03 Ethylene Vinyl Acetate (EVA) Base Conductive Plastic
(Unverified Data**) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |