Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1.86 MPa | 270 psi | |
Pyrotek Pyroboard™ S1300 Roller Pyroboard™ S1300 was developed specifically for use in hotter zones of an annealing furnace.Information provided by Pyrotek. |
|||
Tensile Strength, Ultimate | 1.86 MPa | 270 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength, Ultimate | 1.86 MPa | 270 psi | |
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Tensile Strength, Ultimate | 1.86 MPa | 270 psi | |
Momentive Performance Materials RTV160 White Adhesive Sealant, Non-Corrosive Pourable One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Non-corrosive prote.. |
|||
Tensile Strength, Ultimate | 1.86 MPa | 270 psi | |
Momentive Performance Materials RTV5812 White Adhesive Sealant, Fast Cure Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes.. |
|||
Tensile Strength, Ultimate | 1.86 MPa | 270 psi | |
Momentive Performance Materials RTV5813 Black Adhesive Sealant, Fast Cure Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes.. |
|||
Tensile Strength, Ultimate | 1.86 MPa | 270 psi | |
Momentive Performance Materials RTV5818 Translucent Adhesive Sealant, Fast Cure Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes.. |
|||
Tensile Strength, Ultimate | 1.86 MPa | 270 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |