Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1.32 - 60.0 MPa | 191 - 8700 psi | Average value: 19.0 MPa Grade Count:22 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |