Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1.08 - 28.0 MPa | 157 - 4060 psi | Average value: 9.90 MPa Grade Count:31 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini.. |
|||
Tensile Strength, Ultimate | 1.08 MPa | 156 psi | JIS K6301 |
Stellarchem AB835EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |