Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 8.50 - 11.8 J | 6.27 - 8.70 ft-lb | Average value: 9.88 J Grade Count:4 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Falling Dart Impact | 8.50 - 11.8 J | 6.27 - 8.70 ft-lb | Average value: 9.88 J Grade Count:4 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |