Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 9.93 J | 7.32 ft-lb | ASTM D3763 |
LNP Thermocomp® QF-1006 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Falling Dart Impact | 9.93 J | 7.32 ft-lb | ASTM D3763 |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement