Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 8.50 J | 6.27 ft-lb | ASTM D3763 |
LNP Stat-Kon® PDX-E-99550 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Falling Dart Impact | 8.50 - 11.8 J | 6.27 - 8.70 ft-lb | Average value: 9.88 J Grade Count:4 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Falling Dart Impact | 8.50 - 11.8 J | 6.27 - 8.70 ft-lb | Average value: 9.88 J Grade Count:4 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Falling Dart Impact | 8.50 J | 6.27 ft-lb | ASTM D3763 |
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |