Polymer Property : Falling Dart Impact = 29.16 ft-lb
Polymer Property :
Falling Dart Impact =
29.16 ft-lb
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Falling Dart Impact
>=
39.54
J
>=
29.16
ft-lb
-30°F; ASTM D3029
Spartech Formalloy LG Low-Gloss TPO Alloy Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.