Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 27.1 J | 20.0 ft-lb | 73°F; ASTM D3029 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
Spartech SP-9070 ABS/PVC Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM 3029 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM D5420 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM 3029 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM D5420 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM 3029 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM 3029 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM D5420 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM 3029 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM D5420 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM D5420 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM D5420 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Falling Dart Impact | 27.1 J @Temperature -40.0 °C |
20.0 ft-lb @Temperature -40.0 °F |
ASTM 3029 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |