Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 3.80 J | 2.80 ft-lb | ASTM D3763 |
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |